A silicon carbon anode produced by depositing silicon onto a biologically sourced carbon scaffold. The porous bio-carbon matrix provides internal void space for silicon expansion, limiting stress transfer outward from the particle. It offers a strong combination of 1942.5 mAh/g capacity and 93.8% initial coulombic efficiency.
| Particle Size (D10) | 4.4 um |
| Particle Size (D50) | 7.5 um |
| Particle Size (D90) | 12.6 um |
| Tap Density | 0.9 g/cm³ |
| Specific Surface Area (SSA) | 1.9 m²/g |
| Capacity | 1942.5 mAh/g |
| Initial Efficiency (ICE) | %93.8 |