A nickel-based lithium supplementation additive. At ≥400 mAh/g charge capacity it releases less lithium than LFO, but its low surface area of ≤0.60 m²/g and magnetic substance content of ≤1.0 ppm mean more stable behavior in the electrode slurry and a lower contamination risk.
| Specific Surface Area (SSA) | ≤ 0.60 m²/g |
| Particle Size (D50) | 15.0 ± 2.0 um |
| pH | ≤ 12.30 |
| Magnetic Substances | ≤ 1.0 ppm |
| Residual Alkali (LiOH) | ≤ %5.0 |
| Residual Alkali (Li2CO3) | %2.0 |
| Charge Capacity | ≥ 400 mAh/g |