A fine-grade version of the NCM811 composition at 4.5 microns. Reducing particle size in high-nickel cathodes both improves rate performance and facilitates the transition to a single crystal structure. At 92.4% it has the highest initial coulombic efficiency in the series.
| Lithium (Li) | %7.15 ± 0.30 wt |
| Nickel (Ni) | %49.80 ± 1.5 wt |
| Cobalt (Co) | %7.40 ± 0.60 wt |
| Manganese (Mn) | %2.90 ± 0.60 wt |
| Particle Size (D50) | 4.5 ± 1.5 um |
| Capacity | 209.8 mAh/g |
| Initial Efficiency (ICE) | %92.4 |