The highest-nickel cathode material in this catalog at 94% nickel, delivering 230.8 mAh/g capacity and 93.0% initial coulombic efficiency. At this nickel level cobalt is reduced to 5% and manganese to 1%. Its high performance requires careful protection from contact with moisture and air.
| Nickel (Ni) | %94.0 ± 1.0 mol |
| Cobalt (Co) | %5.0 ± 1.0 mol |
| Manganese (Mn) | %1.0 ± 1.0 mol |
| Particle Size (D50) | 10.23 um |
| Capacity | 230.8 mAh/g |
| Initial Efficiency (ICE) | %93.0 |